Cellophane, Rayophane Regenerated Cellulose Film
Subcategory: Cellulosic; Polymer
Material Notes: General Description:All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by its earliest brand name Cellophane®. The latter films are plasticised by glycols and water to overcome their brittleness and are transparent, colourless and of moderate crystallinity. They were very widely used for packaging but have been substantially replaced by synthetic thermoplastics, especially polypropylene. They have very high permeability to moisture and, especially when dry, very low permeabiltiy to permanent gases. Their moisture content varies greatly with their environment reaching approximately 50% at 100% relative humidity. Not surprisingly, this causes many of their properties to vary considerably - so summarised values must be treated with considerable caution. Information provided by Goodfellow.
| Available Properties |
- Density
- Water Absorption
- Moisture Vapor Transmission
- Oxygen Transmission
- Nitrogen Transmission
- Carbon Dioxide Transmission
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Tensile Modulus
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Specific Heat Capacity
- Thermal Conductivity
- Oxygen Index
- Chemical Resistance - Alkalis
- Chemical Resistance - Dilute Acids
- Chemical Resistance - Greases and Oils
- Permeability to Carbon Dioxide @25°C
- Permeability to Hydrogen
- Permeability to Hydrogen @25°C
- Permeability to Nitrogen @25°C
- Permeability to Oxygen @25°C
- Permeability to Water @25°C
- Radiation Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|