Cellophane, Rayophane Regenerated Cellulose Fiber

 

Subcategory: Cellulosic

Material Notes:
General Description:

All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by its earliest brand name Cellophane®. The latter films are plasticised by glycols and water to overcome their brittleness and are transparent, colourless and of moderate crystallinity. They were very widely used for packaging but have been substantially replaced by synthetic thermoplastics, especially polypropylene.

They have very high permeability to moisture and, especially when dry, very low permeabiltiy to permanent gases. Their moisture content varies greatly with their environment reaching approximately 50% at 100% relative humidity. Not surprisingly, this causes many of their properties to vary considerably - so summarised values must be treated with considerable caution.

Information provided by Goodfellow.

Available Properties
  • Density
  • Water Absorption
  • Tenacity
  • Elongation at Break
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Oxygen Index
  • Chemical Resistance - Alkalis
  • Chemical Resistance - Dilute Acids
  • Chemical Resistance - Greases and Oils
  • Radiation Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。