Greene Tweed CHEMRAZ® 504 Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatures. Chemraz 504 seals effectively in temperatures ranging from -22°F to 446°F (-30°C to 230°C). Chemraz 504 is well suited for a variety of applications, from mechanical seals to valve housings.Chemraz 504 is available for use as O-rings, gaskets and many other custom shapes. Because of its versatility, Chemraz 504 is often used as a standard compound and can be found in a variety of fluids and solutions including acids, caustics, aldehydes, esters, aromatics, hot water, steam, amines, methanol, ketones, TBA and MTBE Applications: - Mechanical seals
- Valves
- Pump Housings
- Sampling/metering equipment
- Reactors
- Mixers
- Controls/instrumentation
- Sprayers/dispensers
- Couplings
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|