Greene Tweed CHEMRAZ® 520 Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Chemraz® 520 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contaminations is required. Additionally, Chemraz 520 offers excellent performance history in static and dynamic plasma and diffusion processes as well as static photolithography processes. Chemraz 520 is formulated for use in high sealing load applications and where temperatures do not exceed 240°C (464°F). Due to the hardness of this material, low-temperature applications may require smoother hardware surface finishes of 10 micro inches (Ra) and below.Applications: - Door seals
- Slit valves
- Isolator valve seats
- Lid Seals
- Gas inlet seals
- KF fitting seals
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|