Greene Tweed CHEMRAZ® 550 Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in dynamic or static processing equipment applications with service temperatures up to 210°C (410°F).Applications: - Valve seals
- Fitting and union seals
- Gaskets
- Regulator seals
- Filter seals
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|