Greene Tweed CHEMRAZ® 605 Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Chemraz® 605, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. A high temperature compound with superior compression set resistance, physical properties and excellent chemical resistance, it excels in demanding static and semi-dynamic applications. Chemraz 605 exhibits unparalleled performance with hot amines, steam and water and functions well in increased temperatures ranging from -4°F to 500°F (-20°C to 260°C).Available in O-rings, gaskets and many other custom shapes, Chemraz 605 possess a broad chemical resistance range. The 605 compound is suitable for use in a wide variety of media including acids, caustics, aldehydes, esters, ethers, aromatics, hot water, steam, amines, methanol, ketones, TBA ad MTBE. Applications: - Mechanical seals
- Valves
- Pump Housings
- Sampling/metering equipment
- Compressors
- Reactors
- Mixers
- Controls/instrumentation
- Sprayers/dispensers
- Couplings
- Diaphrams
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|