Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Chemraz® is a black perfluoroelastomer specifically formulated to meet the extreme demands of diffusion, LPCVD and thin dry processing applications. It exhibits superior compression set resistance and is recommended for static and dynamic high temperature applications up to 324°C (615°F).Applications: - Quartz rod seals
- Bell jar seals
- High-temperature valve seals
- KF fitting seals
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|