Greene Tweed CHEMRAZ® SD585 Perfluoroelastomer

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Material Notes:
Chemraz® SD 585, a cream-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance similar to PTFE. Because it offers the best low-temperature sealing properties of a perfluoroelastomer on the market, Chemraz is an ideal seal component for sub ambient mechanical seal applications. Chemraz SD585 is recommended for strong oxidizing media an hot aqueous solutions

Chemraz SD585’s many features make it well suited for critical applications and difficult seal replacement locations where maximizing MTBR (meant time between replacement) is paramount. With its cream color, Chemraz SD585 meets the needs of applications requiring non-black elastomers

Chemraz components are available for use as O-rings, gaskets, sanitary seals and many other custom shapes

This product is FDA and USP Class VI compliant making it an ideal product for elastomeric applications requiring regulatory compliance.

Applications:

  • Mechanical seals
  • Valves
  • Pumps
  • Mixers
  • Fermenters
  • Biomedical equipment
  • Couplings

Information provided by Green Tweed

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • Tensile Modulus
  • Compression Set
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。