Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Chemraz® SD625, a black-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance and low extractables similar to PTFE. Not only is it FDA and USP Class VI compliant, but Chemraz SD625 also passes USP Physicochemical Testing, USP <661>, and has been tested to USP elastomeric closures, USP <381>, making it the most comprehensively tested perfluoroelastomer on the market. Critical applications and difficult seal replacement locations where maximizing MTBR (mean time between replacement) is paramount will benefit greatly from Chemraz SD 625.With is outstanding performance in high temperatures, Chemraz SD625 delivers excellent performance in hot water and steam and in CIP/SIP processes. Chemraz SD625 is also well suited for dynamic applications Chemraz components are available for use as O-rings, gaskets, sanitary seals and many other custom shapes. Applications: - Mechanical seals
- Valves
- Pumps
- Mixers
- Fermenters
- Biomedical equipment
- Couplings
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|