Greene Tweed AR™ HT Abrasive-Resistant Thermoplastic

 

Subcategory: Thermoplastic

Material Notes:
ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outstanding chemical, thermal shock and impact resistance, making it a better wear material than traditional rubber, ceramic or bronze materials.

Greene Tweed’s proprietary AR thermoplastic materials exhibit outstanding wear characteristics in media containing solids. AR combines excellent abrasive resistance, good dry run capability and superior vibration dampening characteristics with no hydrolysis or swell.

ARHT works well in a variety of abrasive pump applications iuncluding those working with sirculatiing water, open and closed cooling water, river water, screen wash and crude oil pumps. When using ARHT pump users can operate their equipment with much tighter clearances, boosting efficiency and improving process reliability.

Applications:

  • Circulating water pumps
  • Crude oil multistage pumps
  • Open and closed cooling water pumps
  • River water pumps
  • Screen wash pumps
  • Sump pumps

Information provided by Green Tweed

Available Properties
  • Specific Gravity
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • CTE, linear, 212°F (100°C)
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。