Greene Tweed AR™ HT Abrasive-Resistant Thermoplastic
Subcategory: Thermoplastic
Material Notes: ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outstanding chemical, thermal shock and impact resistance, making it a better wear material than traditional rubber, ceramic or bronze materials.Greene Tweed’s proprietary AR thermoplastic materials exhibit outstanding wear characteristics in media containing solids. AR combines excellent abrasive resistance, good dry run capability and superior vibration dampening characteristics with no hydrolysis or swell. ARHT works well in a variety of abrasive pump applications iuncluding those working with sirculatiing water, open and closed cooling water, river water, screen wash and crude oil pumps. When using ARHT pump users can operate their equipment with much tighter clearances, boosting efficiency and improving process reliability. Applications: - Circulating water pumps
- Crude oil multistage pumps
- Open and closed cooling water pumps
- River water pumps
- Screen wash pumps
- Sump pumps
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- CTE, linear, 212°F (100°C)
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|