Greene Tweed WR™ 300 PEEK, Carbon Filled
Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer
Material Notes: WR®300 is a carbon-fiber reinforced compression molded PEEK™ often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in clean, lubricated and/or moist environments.WR300 allows the pump user to increase pump efficiency by running tighter wear ring clearances while decreasing potential pump damage when pumps are cavitated or experience radial bearing failures. Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Hardness, Rockwell M
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- CTE, linear, 212°F (100°C)
- Deflection Temperature at 1.8 MPa (264 psi)
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|