Greene Tweed WR™ 525 PEEK, Carbon Filled
Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer
Material Notes: WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK™ matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and case wear rings.WR 525 allows the pump user to increase pump efficiency by running tighter wear ring clearances, while decreasing potential pump damage when pumps are cavitated or experience down-line bearing failures. Information provided by Green Tweed
| Available Properties |
- Tensile Strength @ Yield
- Tensile Modulus
- Compressive Strength
- Compressive Modulus
- Color
|
|
|
|
| Property Data |