Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled
Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer
Material Notes: WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK™ matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material ideal for axial thrust and face loading applications. WR575 provides superior wear characteristics, enabling users to extend mean time between repairsInformation provided by Green Tweed
| Available Properties |
- Specific Gravity
- Tensile Strength @ Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Compressive Modulus
- Color
|
|
|
|