Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber
Subcategory: Polyketone; Thermoplastic; Polymer
Material Notes: Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Orthtek WF components work well as metal replacements due to Orthtek’s high strength, low weight, corrosion resistance, and dimensional stability. Orthtek WF is recommended for applications such as nail guides and retractors where radiolucentcy and autoclaving are required.Applications: - Medical Trauma – External fixation and targeting devices
- Medical Orthopedic – Reconstructive components, retractors, spine instrumentation and surgical instrumentation
Information provided by Green Tweed
| Available Properties |
- Specific Gravity
- Water Absorption
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Compressive Modulus
- Color
- Fiber Orientation
- Fiber Tow Size
- Fiber Volume, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|