Greene Tweed Xycomp® 1030-02 Carbon/Nylon 12 Composite
Subcategory: Nylon; Nylon 12; Polymer
Material Notes: Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific strength and specific stiffness values over 400 percent that of Titanium and superior chemical compatibility and fire resistance properties, Greene, Tweeds Xycomp composites deliver greater value. Like all Greene, Tweed products, Xycomp components reflect the combination of engineering expertise with customer specifications. Additional benefits offered by Xycomp include improved chemical resistance, increased impact, toughness and ductility, more complex single-mold components, excellent post-molding machinability, recyclability, and infinite shelf life.
| Available Properties |
- Specific Gravity
- Tensile Strength @ Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|