EMS-Grivory Grilamid L20HL Sz9563 Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Key Words: Polyamide 12
Material Notes: Data provided by EMS-Grivory. Polyamide-12 medium viscosity injection molding and extrusion grade, heat stabilized. Good chemical resistance, dimensional stability and toughness, exceptional UV stability and termite resistance. Applications: For electrical applications such as cable sheathings.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|