EMS-Grivory Grilon A28GM Nylon 6, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Normal viscosity, nucleated Polyamide-6, injection molding type. A universally applicable injection molding type, easily flowing, impact resistant with good sliding friction characteristics. Applications: Wide variety of applications in all market sectors: car, electrical, leisure and sport. E.g. perfume bottle caps, buttons, clips, covers, housings, etc.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|