EMS-Grivory Grilon BT40Z Nylon 6, As Conditioned

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Key Words: Polyamide 6

Material Notes:
Data provided by EMS-Grivory.

A polyamide blend with amorphous and semi-crystalline constituents; injection molding types. Characterized by the combination of high impact resistance with high rigidity. It has higher values than PA6 and PA66. Its low water absorption enhances the dimensional stability and functional safety of finished parts.

Applications: Gear wheels, machine covers, electrical components, in-car electrical/electronic components, etc.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • CTE, linear 20°C Transverse to Flow
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。