EMS-Grivory Grilon CR9 Nat6361 Nylon Copolymer, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 612
Key Words: CoPA; Polyamide Copolymer; Polyamide 612
Material Notes: Data provided by EMS-Grivory. High viscosity CoPA. BGA approved for direct contact with foodstuffs. FDA approved for indirect contact with foodstuffs < 49°C. Product for extrusion applications (single and multi-layer), such as blister and flat films, low curl, good shrinking properties and good blow molding stability, extrusion and blow-molding applications. Applications: Base films, cling/shrink wrap films, pouch films (sealed edge), hollow shapes.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity Test
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|