EMS-Grivory Grilon ELX23NZ Polyether Block Amide (PEBA), Dry As Molded
Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Thermoplastic
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Thermoplastic polyamide elastomer, without plasticizer. Flexible injection molding and extrusion product with good impact strength, even at low temperatures. Applications: Mountain, ski and hiking boots. Hydraulic and pneumatic pipes.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|