EMS-Grivory Grilon PK-5H Nylon 6, 50% glass beads, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Normal viscosity PA6 injection molding type with 50% glass beads, heat stabilized. Injection molded type filled with 50% glass beads, characterized by dimensional precision, impact strength and resistance to warping. Applications: Rigid, warp resistant parts in various sectors. Parts in the engine cooling system, door mirrors, control components, domestic appliances, vehicle parts.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|