EMS-Grivory Grilon PV-25H HM Nylon 6, 25% glass fiber reinforced, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Normal viscosity 25% glass fiber reinforced Polyamide-6 injection molding grade with special modification for injection welding/bonding with SEBS and PP/EPDM alloys. Grilon XE 3278 can be combined with Shore A elastomers. Applications: Automotive plugs and seals, counter wheel sensors (sealing to the cable), housings with integrated switch membranes, grip handles, housings for electro power tools with vibration damping.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|