EMS-Grivory Grilon PVZ-3H Nylon 6, 30% glass fiber reinforced, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Normal viscosity PA6, impact resistant, heat stabilized. 40% glass fiber reinforced injection molding type. The use of an impact resistant modifier provides increased loadability for impact stress. With 30% glass fiber reinforcement, Grilon PVZ-3H is stiff and impact resistant. Applications: A rigid and impact resistant PA6 modified with glass fibers is suitable for many applications. Furniture: structural components. Electric hand-tools: insulated bodies. Sports industry: ski-ties. Automotive industry: strip moldings & electrical parts.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|