EMS-Grivory Grilon R47HW Nylon 6, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Medium viscosity, flexible PA6 extrusion type. Heat stabilized. Flexible Polyamide-6, heat stabilized, can be processed on conventional polyamide tubing and semi-finished product systems. It is characterized by good impact strength even at low temperature. Applications: Co-extruded fuel lines, freon tubes, refrigerant tubes in deep-freeze equipment, vulcanization cores.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Melt Flow
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|