EMS-Grivory Grivory GV-6H Nylon Copolymer, 60% glass fiber reinforced, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6/66; Polymer
Key Words: Polyamide 6/66
Material Notes: Data provided by EMS-Grivory. 60% glass fiber reinforced injection molding grade with partially aromatic polyamide matrix, approved for food contact according to EEC 128/90. Problem free processing results in reduced abrasion compared to other reinforced thermoplastics. Stiff with high strength even after water absorption, dimensionally very stable, low swelling, good surface finish, chemically resistant. Applications: Highly loaded, rigid, dimensionally stable components such as measuring instruments, functional components in automotive and electric industries. Precision components (coil, fat and detergent resistant), gear box housings, nuts and bolts.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|