EMS-Grivory Grilamid® L20 GM Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L20GM is a medium viscosity, fast cycling grade of nylon 12. Lubricated and heat stabilized, it has been developed specifically for applications where high production rates are demanded, and for parts with complex shapes or very long flow paths. Grilamid L20GM can be processed simply and economically into complicated injection molded parts, such as gears, seals, transmission components and ball bearing cages. Grilamid L20GM offers low moisture absorption, thus providing excellent dimensional stability with mechanical properties virtually unaffected by environmental humidity. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|