EMS-Grivory Grilamid® L20 HV1 Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L20 HV1 is an adhesive resin developed for use as a tie layer in multi layer fuel tubes. Specifically designed to adhere Grilamid L25W40X with fluoropolymers, its high adhesion strength is generated during the extrusion process, eliminating the need for post treatment.Information provided by EMS-Grivory
| Available Properties |
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Processing Temperature
- Front Barrel Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |