EMS-Grivory Grilamid® L20 LF Nylon 12, 12% Graphite Filled, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Grilamid L20 LF is a uniquely formulated extrusion grade of nylon 12 containing 12% graphite. The graphite increases lubricity, thereby decreasing the coefficient of friction. This material is easy to from, with good flexibility and kink resistance. Nylon 12 resins such as Grilamid L20 LF offer the lowest moisture absorption of any commercially available nylons, thus providing excellent dimensional stability with mechanical properties virtually unaffected by environmental humidity. Information provided by EMS-Grivory
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Coefficient of Friction
- Izod Impact, Notched
- Izod Impact, Notched @ -40°C
- Melting Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Head Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|