EMS-Grivory Grilamid® L25 Natural 6112 Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L 25 natural 6112 is a high viscous, rigid Polyamide 12 extrusion grade which contains an organic heat stabilizer. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378 (Polyamide tubing for motor vehicles), Type PA12-H. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Tensile Modulus
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Head Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|