EMS-Grivory Grilamid® L25 ANZ Nylon 12, Dry As Molded

 

Subcategory: Nylon; Thermoplastic; Nylon 12

Material Notes:
Grilamid L25 A NZ is a high viscous extrusion blow molding polyamide 12. Due to its good melt strength blow molded articles with volumes up to 50 liters can be processed.

Designed for automotive applications, Grilamid L25 A NZ has exceptionally good hydrolytic stability, and exhibits resistance to zinc chloride, hot water and antifreeze solutions. Compared to PA6 and PA66 resins, the working life of Grilamid L25 A NZ (when in contact with antifreeze) is significantly longer.

Grilamid L25 A NZ has been developed for applications where other polymers, such as polyolefins or PA6 reach their performance limits. Possible applications are flexible fuel filler necks or rigid pipes for automobile cooling systems.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。