EMS-Grivory Grilamid® L25 ANZ Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L25 A NZ is a high viscous extrusion blow molding polyamide 12. Due to its good melt strength blow molded articles with volumes up to 50 liters can be processed. Designed for automotive applications, Grilamid L25 A NZ has exceptionally good hydrolytic stability, and exhibits resistance to zinc chloride, hot water and antifreeze solutions. Compared to PA6 and PA66 resins, the working life of Grilamid L25 A NZ (when in contact with antifreeze) is significantly longer. Grilamid L25 A NZ has been developed for applications where other polymers, such as polyolefins or PA6 reach their performance limits. Possible applications are flexible fuel filler necks or rigid pipes for automobile cooling systems. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|