EMS-Grivory Grilamid® L25FVS40 Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L25FVS40 is a grade of nylon 12 which is modified to provide high flexibility with good tensile strength. Heat and light stabilized, it provides exceptional retention of properties even after prolonged exposure to outdoor weathering and high temperatures. Grilamid nylon 12 resins offer the lowest moisture absorption of any commercially available nylon, thus providing excellent dimensional stability with mechanical properties virtually unaffected by environmental humidity. Grilamid L25FVS40 is supplied in natural and black only, and was specifically developed for fuel and vent line applications. Other applications include extruded flexible tubing and profiles. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Head Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|