EMS-Grivory Grilamid® L25W20X Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L25W20X is a new semi-rigid Polyamide 12 grade with a high cold impact strength and high burst pressure. It is heat and light-stabilized. Designed for Air brake applications, Grilamid L25W20X offers an unusual combination of mechanical properties, providing outstanding flexibility and toughness, even at low temperatures. It meets the requirements of several automotive industry standards; DIN 74323, DIN 74324, ISO 7628 and NF12632 (10 and 12.5 bar). Applications: semi-rigid, cold-impact resistant, UV and heat stabilized tubings for applications in the automotive industry, such as air brake lines, fuel and vent lines, vacuum lines, hydraulic hoses and pneumatic hoses. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Izod Impact, Notched @ -40°C
- Comparative Tracking Index
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|