EMS-Grivory Grilamid® L25W40 ESD Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L 25 W 40 ESD is an anti-static PA 12 compound. This polymers is electrically conductive, making it especially suitable for applications which are in permanent contact with fuel. Grilamid L 25 W 40 ESD black is an unreinforced PA 12 type which is mainly used in extrusion processing applications. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Volume Resistivity
- Surface Resistance
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |