EMS-Grivory Grilamid® L25W40NZ 844 Nylon 12, Dry As Molded

 

Subcategory: Nylon; Thermoplastic; Nylon 12

Material Notes:
Grilamid L25W40NZ 844 is a nylon 12 that is modified to provide high flexibility and excellent toughness, especially at low temperatures. With exceptionally low specific gravity, it provides weight savings and lower volume cost.

Tubing processed with Grilamid L25W40NZ 844 meets the requirements of SAE J844d in all specified dimensions, of the ISO-draft N173E, and several national and automotive company specifications for air brake tubing in automotive applications.

Grilamid L25W40NZ 844 offers an unusual combination of mechanical properties, providing outstanding flexibility and toughness, even at low temperatures, with good tensile strength. Heat and light stabilized, It provides exceptional retention of properties, even after prolonged exposure to outdoor weathering and high temperatures.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Izod Impact, Notched @ -40°C
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。