EMS-Grivory Grilamid® L25W40X Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid L25W40X is a nylon 12 which is modified to provide high flexibility and excellent toughness, especially at low temperatures. With exceptionally low specific gravity, it provides weight savings and lower volume costs. Tubing processed with Grilamid L25W40X meets the requirements of SAE J844d in all specified dimensions of the ISO-draft N173E, and several national and automotive company specifications for air brake tubing in automotive applications. Grilamid L25W40X offers an unusual combination of mechanical properties, providing outstanding flexibility and toughness, even at low temperatures, with good tensile strength. Heat and light stabilized, it provides exceptional retention of properties even after prolonged exposure to outdoor weathering and high temperatures. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|