EMS-Grivory Grilamid® LC-3H Nylon 12, 30% Carbon Fiber Filled, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Grilamid LC-3H is a PA 12 compound for injection molding reinforced with 30% carbon fibers. Polyamide 12 is a polycondensation product of Laurinlactam. Compared to other polyamides it has the lowest water absorption and the lowest raw density. The carbon fiber reinforced Grilamid LC-3H is only available in black. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Coefficient of Friction
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|