EMS-Grivory Grilamid® LKN-5H Nylon 12, 50% Glass Bead Filled, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Grilamid LKN-5H is a 50% glass bead reinforced , heat stabilized grade of nylon 12, formulated specifically for applications requiring toughness and rigidity. Stabilized for protection against thermal degradation, Grilamid LKN-5H offers excellent wear and abrasion performance and superior chemical resistance. Grilamid nylon 12 resins offer the lowest moisture absorption of any commercially available nylon, thus providing excellent dimensional stability with mechanical properties virtually unaffected by environmental humidity. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|