EMS-Grivory Grilamid® LKN-5H Nylon 12, 50% Glass Bead Filled, As Conditioned

 

Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer

Material Notes:
Grilamid LKN-5H is a 50% glass bead reinforced , heat stabilized grade of nylon 12, formulated specifically for applications requiring toughness and rigidity. Stabilized for protection against thermal degradation, Grilamid LKN-5H offers excellent wear and abrasion performance and superior chemical resistance.

Grilamid nylon 12 resins offer the lowest moisture absorption of any commercially available nylon, thus providing excellent dimensional stability with mechanical properties virtually unaffected by environmental humidity.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Strength
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。