EMS-Grivory Grilamid® LV-3AH Nylon 12, 30% Glass Fiber Filled, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Grilamid LV-3AH is a 30% glass fiber reinforced PA12 suitable for injection molding. A low density, high impact material, Grilamid LV-3AH also offers excellent hydrolysis resistance, high stress crack resistance, high chemical resistance and high electrical resistance values.Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|