EMS-Grivory Grilamid® LV-23 ESD Nylon 12, 23% Glass Fiber Filled, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Grilamid LV-23 ESD is a carbon and glass fiber reinforced, heat stabilized, molding grade of nylon 12. It is formulated specifically for applications requiring dissipation of static charges and is stabilized for protection against both thermal and UV degradation. Grilamid LV-23 ESD offers excellent wear and abrasion performance and superior chemical resistance. Grilamid nylon 12 resins offer the lowest moisture absorption of any commercially available nylon, thus providing excellent dimensional stability with mechanical properties virtually unaffected by environmental humidity. Grilamid LV-23 ESD can be simply and economically processed into complicated injection molded parts. Some applications include antistatic high strength parts for automotive fuel connectors, fuel rails and snap-fit connectors. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Sourgas-Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|