EMS-Grivory Grilamid® TR55 Transparent Nylon 12, Dry As Molded

 

Subcategory: Nylon; Thermoplastic; Nylon 12

Material Notes:
Grilamid TR 55 is a uniquely versatile material. Based on Nylon 12, Grilamid TR 55 combines’ excellent transparency with superior chemical resistance, strength, stiffness, toughness and outstanding process ability.

Transparency at any processable wall thickness is achievable with Grilamid TR 55. The excellent transparency is maintained even after prolonged exposure to boiling water. Grilamid TR 55 is NSF Standard 61 Listed and also complies with the requirements of CFR 21 Part 177, Section 1500 for nylon 12T resins in direct contact with food.

Typical applications for Grilamid TR 55 are fuel, air or water filter bodies, faucet and shower handles, electrical/electronic components and automotive parts.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Refractive Index
  • Haze
  • Transmission, Visible
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Die Temperature
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。