EMS-Grivory Grilamid® TR55 Transparent Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid TR 55 is a uniquely versatile material. Based on Nylon 12, Grilamid TR 55 combines’ excellent transparency with superior chemical resistance, strength, stiffness, toughness and outstanding process ability. Transparency at any processable wall thickness is achievable with Grilamid TR 55. The excellent transparency is maintained even after prolonged exposure to boiling water. Grilamid TR 55 is NSF Standard 61 Listed and also complies with the requirements of CFR 21 Part 177, Section 1500 for nylon 12T resins in direct contact with food. Typical applications for Grilamid TR 55 are fuel, air or water filter bodies, faucet and shower handles, electrical/electronic components and automotive parts. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Refractive Index
- Haze
- Transmission, Visible
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|