EMS-Grivory Grilamid® TR55 LX2 Transparent Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid TR 55 LX2 is a modified grade of Grilamid TR 55, providing high practical toughness and resistance to chemicals such as alcohol and cleaning agents. Light and heat stabilized, Grilamid TR 55 LX2 offers excellent retention of properties after prolonged exposure to outdoor weathering and high temperatures. It also offers stress-cracking resistance, dimensional stability and mechanical properties virtually independent of environmental humidity. Originally developed for eyeglass frames (both safety and fashion types), Grilamid TR 55 LX2 may be considered for many other applications in which alcohol resistance, transparency and toughness are desired. Grilamid TR 55 LX2 contains no plasticiser, resists cosmetic chemicals and perspiration, does not irritate the skin and can enhance design and performance of personal care products. Industrial applications include auto parts, sight glasses and extruded tubing, sheet and profiles. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|