EMS-Grivory Grilamid® TR90 Transparent Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid TR 90 is a transparent polyamide with good heat resistance and excellent fatigue behavior. Grilamid TR 90 also exhibits low moisture absorption and dimensional stability. Grilamid TR 90 was developed for use in filter bowls, eye glass frames, tooth brushes and optical fiber containing cables. It may also be considered for a variety of consumer and industrial applications in which chemical resistance, transparency and toughness are desired. Because Grilamid TR 90 contains no plasticizer and resists cosmetic chemicals and perspiration, it can enhance the design and performance of personal products such as sport and safety spectacle frames. Grilamid TR 90 is NSF Standard 61 Listed. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|