EMS-Grivory Grilamid® TR90 LX Transparent Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid TR 90 LX is a transparent and tough thermoplastic engineering polyamide. Grilamid TR 90 LX offers excellent alternate bending strength and stress crack resistance in alcohol, ketone, halogenated and aromatic solvents and peppermint oil. Suitable for injection molding and extrusion, Grilamid TR 90 LX was developed for use in filter bowls, eye glass frames, tooth brushes and optical fiber containing cables. It may also be considered for a variety of consumer and industrial applications in which chemical resistance, transparency and toughness are desired. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|