EMS-Grivory Grilamid® TR90 UV Natural Transparent Nylon 12, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid TR 90 UV natural is a transparent and though material with a very bright color and outstanding weathering stability. It offers a very good alternate bending strength and stress crack resistance. In contact with alcohol, ceatons, halogenated, aromatical solvent and usual automobile liquids or cleansing agent. Grilamid TR 90 UV is especially suited for outside application processed by injection molding. It doesnt tend to tarnish. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Processing Temperature
- Nozzle Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|