EMS-Grivory Grilamid® TR XE3805 Transparent Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid TR XE 3805 is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR XE 3805 is a dedicated material for high quality optical lens applications. Lenses manufactured out of Grilamid TR XE 3805 are in compliance with the Optical Class 1 Standard. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|