EMS-Grivory Grilamid® XE 3691 Nylon 12, Steel and Glass Fiber Filled, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Grilamid XE 3691 is an antistatic polyamide 12 with steel and glass fibers reinforcement. Grilamid XE 3691 is recommended for filter elements and connectors in fuel systems.Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
|
|
|
|